Zhrolls specializes in high-precision cold rolling mill rolls engineered to enhance the performance of rolling mills worldwide. With decades of expertise, we provide customized solutions that optimize steel production efficiency and reduce downtime. Our products are ideal for various mill types, including Single Stand Rolling Mills, Rolling Tandem Mills, Cluster Mills, and Skin Pass Mills.

Why Choose Zhrolls?

Durability & Performance: Our cold rolling mill rolls are made from high-grade materials like 9Cr2Mo, 9Cr3Mo, and other alloy steels, ensuring superior hardness and wear resistance. These rolls can withstand the most demanding conditions, helping your mill operate more efficiently and for longer periods without frequent replacements.

Tailored Solutions: Whether you need work rolls, intermediate rolls, or back-up rolls, Zhrolls offers customization to meet your specific operational needs. Our expert team works closely with clients to design and manufacture the perfect solution for your production processes.

Advanced Technology: Our cold rolling mill rolls are designed according to the latest standards (GB/T13314-2008, JB/T4120-2017), ensuring that they meet or exceed industry expectations for quality and precision.

Cost Efficiency: By improving the longevity and performance of your rolls, Zhrolls helps reduce downtime and maintenance costs, ensuring maximum productivity and cost-efficiency in your operations.

With Zhrolls, you gain access to advanced rolling mill technology and exceptional technical support. Contact us today to learn more about how our solutions can enhance your mill’s efficiency and durability.

Work Rolls Mill Type Single Stand Rolling Mill, Rolling Tandem Mill, Cluster Mill, Skin Pass Mill
Material 9Cr2Mo、9Cr3Mo、9Cr5Mo、W6Mo5Cr4V2(M2)、8Cr3MoV、8Cr5MoV、Cr12Mo1V1 (D2)、Cr12Mo1V1+Co (D2+Co)
Diameter ¢40-¢250*
Length 450mm-1450mm
Hardness of Barrel 75-93 HSD
Hardness of Neck 30-60 HSD
Thickness of hardened layer Harden depth 5-15mm
Execution Standards GB/T13314-2008
Intermediate Rolls Mill Type Single Stand Rolling Mill, Rolling Tandem Mill, Cluster Mill, Skin Pass Mill
Material 5H12、8Cr5MoV
Diameter ¢250-¢450*
Length 500mm-1600mm
Hardness of Barrel 74-82 HSD
Hardness of Neck 40-60 HSD
Thickness of hardened layer Harden depth 10-30mm
Execution Standards GB/T13314-2008
Back-up Rolls Mill Type Single Stand Rolling Mill, Rolling Tandem Mill, Cluster Mill, Skin Pass Mill
Material 45Cr4NiMoV、50Cr5MoV、60CrMnMo、60CrNiMo、70Cr3Mo、70Cr3NiMo
Diameter ¢450-¢1600*
Length 450mm-1780mm
Hardness of Barrel 52-72 HSD
Hardness of Neck 30-55 HSD
Thickness of hardened layer Harden depth 25-55mm
Execution Standards JB/T4120-2017

Various material chemistries

MaterialCSiMnPSCrNiMoVWCo
9Cr2Mo0.85-0.950.25-0.450.20-0.35≤0.025≤0.0251.70-2.10≤0.250.20-0.40
9Cr3Mo0.85-0.950.25-0.450.20-0.35≤0.025≤0.0252.50-3.50≤0.250.20-0.40
9Cr5Mo0.85-0.950.25-0.450.20-0.35≤0.025≤0.0254.80-5.50≤0.250.20-0.40
8Cr3MoV0.78-1.100.40-1.100.20-0.50≤0.025≤0.0252.80-3.20≤0.800.20-0.600.05-0.15
8Cr5MoV0.78-0.900.40-1.100.20-0.50≤0.020≤0.0204.80-5.50≤0.800.20-0.600.10-0.20
M20.80-0.900.20-0.450.15-0.40≤0.025≤0.0253.80-4.404.50-5.501.75-2.205.50-6.75
Cr12Mo1V1(D2)1.40-1.60≤0.60≤0.60≤0.020≤0.01011.00-13.00≤0.150.90-1.100.75-0.95≤0.15
Cr12Mo1V1+Co(D2+Mo).40-1.60≤0.60≤0.60≤0.020≤0.01011.00-13.00≤0.150.90-1.100.75-0.95≤0.150.35-0.50
MaterialCSiMnPSCrNiMoVWCo
5H120.48-0.550.80-1.200.20-0.50≤0.025≤0.0104.80-5.501.0-1.500.30-0.601.0-1.50
8Cr5MoV0.78-0.900.40-1.100.20-0.50≤0.020≤0.0204.80-5.50≤0.800.20-0.600.10-0.20
MaterialCSiMnPSCrNiMoVWCo
45Cr4NiMoV0.40-0.500.40-0.800.60-0.80≤0.020≤0.0203.50-4.500.40-0.800.40-0.800.05-0.15
50Cr5MoV0.40-0.600.40-0.800.50-0.80≤0.020≤0.0204.50-5.50≤0.600.40-0.80≤0.30
70Cr3Mo0.60-0.750.40-0.700.50-0.90≤0.025≤0.0252.0-3.50≤0.600.25-0.60